http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003159562-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-02 |
filingDate | 2001-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05635c37f8bc83ccef0b748cc1a094bb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_abd0370f0787bc2a181bf768bf8b2c0e |
publicationDate | 2003-06-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003159562-A |
titleOfInvention | Method for producing painted resin molded product and molded product |
abstract | (57) [Summary] An object of the present invention is to efficiently perform surface treatment such as deburring and coating of a thermoplastic resin molded product obtained by injection molding, and improve the adhesion strength of coating. A blasting material having an average particle size of 150 to 2500 μm is projected onto a thermoplastic resin molded product obtained by injection molding, the molded product is deburred, and the surface of the molded product is JIS-B0601. The center line average roughness Ra measured according to the formula is Ra = 0.3 to 50 μm and the maximum height Rm A method for producing a coated resin molded product, comprising performing a surface treatment so that the relationship with ax is within the range of the following general formula (1), and thereafter applying a paint to the surface. Ra ≦ Rmax ≦ 20 × Ra Formula (1) |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018034229-A1 |
priorityDate | 2001-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 55.