http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003149934-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_01c1e0bc0628f76dea731cda5a666ca1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-08 |
filingDate | 2001-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f7693f4092178933a86f22650fac0b7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9312bbe37e6ac6e68e260eb33da7a005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_565f97b1c6de4121fe84db785f4b74f3 |
publicationDate | 2003-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003149934-A |
titleOfInvention | Developing roller |
abstract | (57) [Summary] [Problem] To effectively reduce odor generated during roller production and suppress aggregation of carbon black at the time of heat-curing the composition, thereby causing variation in resistance between and within samples. Is small, and furthermore, the developing roller has a small resistance fluctuation against environmental changes. An oxyalkylene polymer having at least one hydrosilyl-reactive alkenyl group in a molecule, a compound having at least two hydrosilyl groups in a molecule, a hydrosilylation catalyst, carbon black, and at least one molecule in a molecule are provided. The above object has been achieved by producing a developing roller using a composition comprising a compound containing one acid anhydride unit. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7687559-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2005054372-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2005054372-A1 |
priorityDate | 2001-11-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 86.