http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003147202-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1cca6666104fc82dcac354ff620f4ca http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5419 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D143-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-02 |
filingDate | 2002-08-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3a3f1076331c8de015c6422647065f6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ceac3d9510ec407dc9acf73f2843263d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cdbd6acb861e8d7eded44ea62ea6f0de |
publicationDate | 2003-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003147202-A |
titleOfInvention | Composition containing silicon component and fluorine component and snow and ice prevention member |
abstract | (57) [Problem] To provide a composition containing a silicon component and a fluorine component, which has both an effect of preventing snow accretion and ice at the time of snowfall and at a low temperature and a performance of snow sliding at the time of temperature rise. SOLUTION: At least a specific silicon-containing compound and a fluorine-containing compound are contained, and if necessary, 25 parts by weight or less based on 100 parts by weight (in terms of SiO 2 ) of the above-mentioned specific silicon-containing compound. A composition containing a silicon component and a fluorine component for a coating film or film containing a proportion of another silicon-containing compound, wherein the surface free energy (γ) at 25 ° C. of the coating film or film is 5 2424 [mN / m], and the dispersive force component (γd) and the non-dispersive force component (γ p) is 8.5 to 20 and the rate of increase in surface free energy before and after immersion treatment of this coating film or film at 90 ° C. for 5 minutes is 1. It is within 5 times. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101190955-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015023213-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8753750-B2 |
priorityDate | 2001-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |