http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003128744-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e79b36d234409c330a83cf7956fb4e10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16C13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 |
filingDate | 2001-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab84bbe8200ace6b7bccae895c923d11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b48f97913dc2bef98ec091d7ee8f8d8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6193100ee56f759c286abb1127e08f2b |
publicationDate | 2003-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003128744-A |
titleOfInvention | Formable composition for polyurethane roll and method for producing polyurethane roll using the same |
abstract | PROBLEM TO BE SOLVED: To provide a polyurethane roll-forming composition having low hardness and small compression set, and a method for producing a polyurethane roll using the same. SOLUTION: PPG (a1) and TDI (a) having a nominal number of functional groups of 2 to 3 and a number average molecular weight of 500 to 12,000. 2), a main agent (A) containing an NCO-terminated prepolymer (A1) having an NCO content of 5 to 15% by mass as a main component, a nominal number of functional groups of 2 to 3, and a number average molecular weight of 5 It consists of a hardener (B) containing PTMG (B1) as a main component and having a hardness (type A) of 30 to 12,000. The present invention solves the above problem by a polyurethane-based low-hardness roll-forming composition characterized by being 60, and a polyurethane-based low-hardness roll manufacturing method using the same. |
priorityDate | 2001-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links