http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003098628-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 |
filingDate | 2001-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_12cc6ff6192bd3a4d1ad8c84e3dbfeef |
publicationDate | 2003-04-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003098628-A |
titleOfInvention | Method for producing photothermographic material |
abstract | [57] [Summary] [Problem] To eliminate aggregation of a polymer in an emulsion polymerization system due to contact with a divalent or higher organic acid by eliminating a step or cut-out image on a support, and to reduce the occurrence of streak failure. To provide a method for producing a photothermographic material excellent in manufacturability. A step of winding a transparent support having a thickness of 50 to 250 μm and containing polyester in a roll shape so that the temperature of the transparent support is 40 ° C. or less, and after the winding step, And a step of applying a liquid containing an emulsion polymerization polymer on a transparent support, and a step of applying a liquid containing a divalent or higher organic acid on the transparent support after the winding step. And a method for producing a photothermographic material. |
priorityDate | 2001-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 173.