abstract |
PROBLEM TO BE SOLVED: To provide a linear polycarbonate having improved fluidity, free of deposits on a mold when injection molding is performed, and having good appearance of a molded product. SOLUTION: The viscosity-average molecular weight 1 produced using a long-chain monoalkylphenol having an alkyl group having an average carbon number of 19 to 35 as a terminal terminator and having an unreacted long-chain monoalkylphenol content of 300 ppm or less. 3,500 to 30,000 linear polycarbonates. |