http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003084462-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-05 |
filingDate | 2001-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df6b76fa73cd78bfaa875d5ca69cc1c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff21f70e38a3fae2656579c07eff9957 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9dd21d33dfee7b19201bb2d5bb3572a7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3124ae0aa3da484ad3238dba2590e83 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cffc64a6fd3c3ef60cddc65d020b4cd1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_39c1b29622a859c8a18b29d6b29504b8 |
publicationDate | 2003-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003084462-A |
titleOfInvention | Electrophotographic photoreceptor, method of manufacturing electrophotographic photoreceptor, electrophotographic method, electrophotographic apparatus, and process cartridge for electrophotographic apparatus |
abstract | (57) [Problem] To provide an electrophotographic photoreceptor having excellent abrasion resistance at the time of repeated use, and having less sensitivity deterioration even at the time of repeated use, and having excellent abrasion resistance at the time of repeated use, and Provided are an electrophotographic method, an electrophotographic apparatus, and an electrophotographic process cartridge capable of obtaining stable characteristics with less sensitivity deterioration even when repeatedly used. SOLUTION: At least a charge generation layer 32 is formed on a conductive support 31 and a charge transport layer 33 formed by coating with a charge transport layer coating liquid using a mixed solvent of tetrahydrofuran and anisole or toluene as a coating solvent. Of the residual anisole or toluene with respect to the solid content in the photosensitive layer of the electrophotographic photosensitive member having the photosensitive layer 34 composed of 0 to 50,000 ppm. The drying temperature of the charge generation layer is set to 90 to 120C. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008216999-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008099740-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011123089-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016142754-A |
priorityDate | 2001-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 75.