Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L81-02 |
filingDate |
2001-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ccd3d57065a9be541377feaf8478cb03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e0c59040ed042faf0fe1b4f5f01eb5b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bb942610eae9829dfae3e0b8960ea779 |
publicationDate |
2003-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2003064258-A |
titleOfInvention |
Polyarylene sulfide resin composition |
abstract |
(57) [Summary] [Problem] Without greatly impairing the original excellent characteristics, Provided is a polyarylene sulfide resin composition that reduces the amount of burrs generated and has excellent melt fluidity. SOLUTION: (a) Apatite compound is added in an amount of 5-1 to 100 parts by weight of a polyarylene sulfide resin. A polyarylene sulfide resin composition containing 00 parts by weight. |