Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-038 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L35-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 |
filingDate |
2001-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0fad34bd5f4161fe9b706c1757095dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_89739e27edeae7c59079acc045c0d01b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4903f8b3f758ad39b1af7a7ff49b5b4c |
publicationDate |
2003-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2003035815-A |
titleOfInvention |
Composition for color filter and color filter |
abstract |
PROBLEM TO BE SOLVED: To provide a color filter composition having high heat resistance and excellent dispersibility as well as good developability, and a color filter having high color purity produced using the color filter composition. provide. SOLUTION: The composition for a color filter contains (1) a dispersant, (2) a binder resin and (3) a pigment. The dispersant is an AB block copolymer and / or a BAB block copolymer composed of an A block having a quaternary ammonium group in the side chain and a B block having no quaternary ammonium group. . The binder resin has a light transmittance T at 450 nm of a coating film applied so as to have a thickness of 2.0 μm after heat treatment at 230 ° C. for 30 minutes. 0 (%) and the light transmittance T 1 (%) at 450 nm after heat treatment of the coating film at 230 ° C. for 30 minutes is 1 (%) Or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008156148-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009025820-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012212005-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101129962-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I427414-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I418599-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005126674-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8512921-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012173647-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004339355-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004339330-A |
priorityDate |
2001-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |