Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_026917a1661e94c21035d1c5d1fa135e |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 |
filingDate |
2001-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d1ec687a98723cfb3350e5452d83b2f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_670d5983417f7b054813b02015ef4d67 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c939642481aa076336aa7afd5c18ed9 |
publicationDate |
2003-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2003027397-A |
titleOfInvention |
Forming base paper |
abstract |
(57) [Summary] [PROBLEMS] To have good formability and high productivity by suppressing the occurrence of cracks and folds and wrinkles in a base sheet during press forming, and suppressing cracks and tears on the sheet surface. Further, the present invention provides a molded base paper from which a molded article having excellent strength after press molding is obtained. SOLUTION: The molded base paper mainly composed of natural pulp, which has a basis weight of 100 to 500 g / m 2 and contains an alkyl group-containing compound. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007262603-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007056427-A |
priorityDate |
2001-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |