http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003025043-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7bfb49f41dab1c01cbf6753bc05d8f28 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C9-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-22 |
filingDate | 2001-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e9584f1f400042f1b863cc618e8ac289 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_26925ff3a7e3dd7a2ddec6b4c108905f |
publicationDate | 2003-01-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003025043-A |
titleOfInvention | Casting mold and manufacturing method |
abstract | PROBLEM TO BE SOLVED: To provide a granular aggregate for a mold which gives a high strength to a mold even in a surface state unfavorable due to static electricity and other physical actions, a method for producing a mold, and a mold having a high strength. provide. SOLUTION: A primary agitation mixing step of first adding only a small amount of a polyol component among binder components for a mold to a granular aggregate and stirring and mixing the mixture, and the polyol component and the polyisocyanate component are cured (and, in some cases, cured). A method in which a mold is manufactured by separately performing a secondary stirring and mixing step of simultaneously adding and stirring and mixing the catalyst. |