http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003021713-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-028 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-20 |
filingDate | 2001-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fac2d51a33ba46db3a97cdee5e47ecb5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c405462c940c373198d67d03a7d06f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c41532583b9cb810e1512b884324d060 |
publicationDate | 2003-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003021713-A |
titleOfInvention | Manufacturing method of color filter |
abstract | (57) [Summary] [Problem] To enable a liquid crystal display device with excellent display quality, And the manufacturing method of a color filter with high manufacturing efficiency is provided. The photosensitive resin composition contains at least a polymer, a monomer, and a photopolymerization initiator, the content of the photopolymerization initiator is in the range of 5 to 20% by weight of the solid content, and photopolymerization is started. Between the molar extinction coefficient ε300 at 300 nm and the molar extinction coefficient ε365 at 365 nm, ε300> ε365, ε300 <10000 (I / mol · c m) A photosensitive resin layer is formed using a photosensitive resin composition containing 70% by weight or more of a photopolymerization initiator that satisfies the relationship, and then, as an emission spectrum, g-line, h-line, The photosensitive resin layer is exposed and developed in a predetermined pattern by an exposure apparatus having an i-line and having a spectrum having an energy of 35% or more of the i-line energy in a wavelength range of 290 to 350 nm. Let it be the manufacturing method of the color filter provided with the process of forming the resin layer of the range of 1-3 micrometers. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006109528-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008304688-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005316012-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006134856-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4556479-B2 |
priorityDate | 2001-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 168.