http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003003038-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 |
filingDate | 2001-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_570b49ac22a6e899ce57db7a6aab7453 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c6724400c4c0aae884f296f963b03eb5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f7480b40bfafdbf3c295facfaf5465d2 |
publicationDate | 2003-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2003003038-A |
titleOfInvention | Thermoplastic elastomer composition and method for producing the same |
abstract | (57) [SUMMARY] [PROBLEMS] To provide a flexible, manufacturable process by a simple melt-kneading process. Rubber elasticity at high temperature, mechanical strength, oil resistance, solvent resistance, Provision of a thermoplastic elastomer composition having excellent heat resistance, weather resistance, and surface characteristics. (I) A hydrogenated block copolymer (a) having a vinyl aromatic compound polymer block and a hydrogenated conjugated diene compound polymer block having a number average molecular weight of 200,000 or more, a vinyl aromatic compound polymer block, and A non-hydrogenated block copolymer (b) having a conjugated diene compound polymer block, a non-aromatic rubber softener (c), a peroxide-crosslinked olefin resin (d) having a density of 0.94 g / cm 3 or more, It contains a peroxide-decomposable olefin resin (e), an organic peroxide (f), and a crosslinking aid (g), and the blending ratio of (a) :( b) is 85:15. ~ 99: 1, for 100 parts by mass of (a) and (b) in total, (c) 50 to 250 parts by mass and (d) 2.5 to 50 parts by mass, (e) to (d) A thermoplastic elastomer composition obtained by dynamically cross-linking a mixture blended at 0.5 to 10 times by mass. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019131722-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100904192-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009534485-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7253233-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008174760-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012081561-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015071653-A |