abstract |
PROBLEM TO BE SOLVED: To provide a method for producing a molded article having high short-time thermal shape stability and to provide the molded article. The objectives are: a) 35-100% by weight of a thermoplastic polyester, b) 0-60% by weight of a filler or reinforcing material, c) 0-20% by weight of an elastic rubber for modifying impact strength, d. A) a flame retardant of 0 to 30% by mass, e) a synergist of 0 to 20% by mass, f) other additives and / or a processing aid of 0 to 5% by mass. The problem is solved by storing at a temperature of 180 to 250 ° C. for one hour. |