http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002537112-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-31551 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-577 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D7-574 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 |
filingDate | 2000-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2002-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002537112-A |
titleOfInvention | Multi-layer lacquer coating with high scratch resistance, its production method and its use |
abstract | (57) [Summary] A case containing (A) a base lacquer layer, (B) a first clear lacquer layer as an intermediate layer, and (C) a second clear lacquer layer as an uppermost layer, which are superposed in this order. In the multi-layer lacquer coating with high scratch resistance on a substrate which has been primed according to (1), the second clear lacquer layer (C) has the formula (C1): —O— (CO) —NH 2 —O— (CO) —NH— At least one oligomer and / or polymer having at least one lateral carbamate and / or allophanate group (c11), in particular (C11), of (CO) —NH 2 and (C2) a carbamate group and And / or paint (C) containing at least one crosslinking agent containing at least two functional groups (c21) that undergo a crosslinking reaction with allophanate groups (c11) Method for producing and a multilayer lacquering high scratch resistance; high scratch multilayer lacquering resistor, characterized in that it can et produced. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013166993-A |
priorityDate | 1999-02-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 172.