http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002513338-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S428-913 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10S428-914 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24942 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24802 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-5227 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-382 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-50 |
filingDate | 1998-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2002-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002513338-A |
titleOfInvention | Thermal dye diffusion coatings and substrates |
abstract | (57) [Summary]nA coating suitable for receiving an image by dye diffusion printing comprising a thermoplastic polymer having a glass transition temperature of at least about 30 ° C and a powdered plasticizer having a melting point of at least about 80 ° C. Thermoplastic polymers have a glass transition temperature of at least 40 ° C. For example, the thermoplastic polymer may be a vinyl chloride acrylate copolymer. The plasticizer may be an aromatic carboxylic acid ester such as cycloxane / dimethanol / dibenzoate. The average particle size of the powdered plasticizer is less than about 20 micrometers. The weight ratio of thermoplastic polymer to plasticizer generally ranges from 80:20 to about 40:60. The coating includes a release agent. The release agent may be present in a range from about 0.5 to about 10 weight percent based on the weight of the dry coating. The present invention further provides a coated substrate suitable for receiving an image by dye diffusion printing, a thermoplastic polymer having a glass transition temperature of at least about 30 ° C, a powdered plasticizer having a melting point of at least about 80 ° C, A coating composition is provided which is an aqueous dispersion of a release agent. |
priorityDate | 1997-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |