Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2531-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2231-122 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F36-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-223 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C53-128 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C51-41 |
filingDate |
1999-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2002-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002512249-A |
titleOfInvention |
Stable concentrated liquid rare earth carboxylate |
abstract |
(57) [Summary]nA stable liquid rare earth carboxylate having a high rare earth concentration and suitable for use in forming an active Ziegler-Natta catalyst is prepared using a stabilizing agent such as water and / or an acid Contains from about 45% to about 20% rare earth elements. A novel fabrication method is disclosed. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015013922-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10604602-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022045282-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015533849-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011516642-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017082139-A |
priorityDate |
1998-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |