Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate |
2001-06-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_748855038ea1b1783063696bbdd76232 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e54144850e553d30b8f9dc5101ab969 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d7d1b03fce5f0e00a00bf9926fcb687 |
publicationDate |
2002-12-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002361736-A |
titleOfInvention |
Biaxially oriented polyester film for hard coat |
abstract |
(57) Abstract: To provide a biaxially stretched polyester film for a hard coat capable of improving the flatness after a hard coat. A thermal expansion in the width direction at 50 ° C. to 100 ° C. with respect to 30 ° C. A biaxially stretched polyester film for a hard coat having a ratio of -0.5% to 0.5% and satisfying the following formulas 1 and 2. 10 μm <R <500 μm Formula 1 ΔR / R <0.05 Formula 2 (where R is the film thickness and ΔR is the film thickness variation) |