http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002321313-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2001-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e9d18dba5b5abb5c5372973e4a7b863 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e29a1c5bebd1881a664e9bdfd202ed0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7e6770dcfd6ba12af41b3b238b047b71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51c5f436dbd9a24c4d46c8602ca8f9d0 |
publicationDate | 2002-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002321313-A |
titleOfInvention | Coating substrate and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a coated substrate excellent in gas barrier properties, adhesion to a substrate, transparency, flexibility and printability, and a method for producing the same. SOLUTION: An organic polymer compound having an amino group, A functional group capable of reacting with an amino group and a SiOR 1 group (R 1 is a hydrogen atom or an alkyl group having 1 to 4 carbon atoms) in the molecule, and an organic compound having the general formula (1): R 2 m Si (OR 3 ) n (wherein, R 2 represents an alkyl group having 1 to 4 carbon atoms or an alkyl group having 1 to 4 carbon atoms having a functional group which does not react with an amino group, and R 3 represents a hydrogen atom or 1 carbon atom. To 4 alkyl groups, n is an integer of 1 or more and m + n = When the coating agent obtained from the organosilicon compound and / or its hydrolytic condensate represented by 4) and a solvent is applied to a substrate, dried and aged, the refractive index of the coating layer immediately after drying ( n 1 ) and the refractive index (n 2 ) of the aged coating layer are (n 2 ) / (n 1 ) ≧ 1.2. |
priorityDate | 2001-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |