http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002309058-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-08 |
filingDate | 2001-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2c2588e25e0c63566a341ee584eaaf51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4a8303745e6465fafd2839c0b9b4e51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44e10f48fa33094dc46f1d48aa9f3299 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_947bf88fa7c4352062398b0d568d3b3d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_59a9a24d25f2b126b346501378d02243 |
publicationDate | 2002-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002309058-A |
titleOfInvention | Molded article with excellent flexibility obtained from thermoplastic polymer composition |
abstract | (57) [Abstract] [Problem] Flexibility and elastic recovery (low permanent set characteristics) It is a molded article excellent in shape, the specific thermoplastic polymer composition used to produce it also shape retention under high temperature, And providing molded products excellent in hot melt moldability such as extrusion molding. SOLUTION: A thermoplastic resin (I) obtained by polymerization of a monomer composed of a methacrylate ester and another monomer as an optional component, a monomer containing an acrylate ester and a polyfunctional monomer A thermoplastic polymer composition comprising rubber-like crosslinked particles (II) obtained by copolymerization of a mixture, wherein the mass ratio of (1) (I) / (II) is 40/60 to 10/90, (2) (I) having a number average molecular weight of 30,00 A molded article obtained by thermoforming a thermoplastic polymer composition having an average particle size of 0 or less, (3) an average particle diameter of (II) of 130 nm or less, and (4) at least (II) satisfying a condition of a continuous phase. |