http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002308657-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e3b0a3dbf8d6c9712d86ea1383fd5327
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00086
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2103-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00198
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00672
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02
classificationIPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-12
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B111-70
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-08
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E21D11-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10
filingDate 2002-02-08-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3f709c4f5f13f499e6677415dbe75148
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a837b91a773ad9fc860168a56d96bd2d
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53b2ca3c0ca7fab19ae0f6b9cfaddc18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_54eaa269cd78762c8d0b0b612d951fc4
publicationDate 2002-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2002308657-A
titleOfInvention Quick-hardening material and quick-hardening lightweight filling mortar
abstract PROBLEM TO BE SOLVED: To provide a quick-hardening material and a quick-hardening lightweight filling mortar which are easy to handle with powder and hardly cause gelling even when left in a slurry state for a long time. SOLUTION: Since calcium carbonate and aluminate are mixed in an amount of 1.5 to 6 in a molar ratio of calcium carbonate / aluminate, handling of a quick-hardened material in a powder state is facilitated. Can be. Also, since sodium carbonate was added to the aluminate in a molar ratio of aluminate / sodium carbonate of only 1 to 13, even if the quick-hardening material was left in a slurry state for a long time, the quick-hardening material slurry gelled. The effect of being difficult is obtained.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1613564-A4
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013035701-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1613564-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008162835-A
priorityDate 2001-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14766
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID452716272
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID449845984
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID450414884
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10340
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID448098817
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID23670858
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID453467280
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID25199638
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID10112

Total number of triples: 37.