http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002303953-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 2001-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1fef7c760fc1e2ee4c255680342f7fa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77d0592288a3b52e157a1c227fbea5f9 |
publicationDate | 2002-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002303953-A |
titleOfInvention | Heat-developable image recording material |
abstract | (57) [Problem] To provide a heat-developable image recording material excellent in both image storability and processing brittleness. A heat-developable image recording material comprising at least one photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent for silver ions, and a binder on one surface of a support. , As the binder, the solization ratio is 5 55% by mass, and the mass average molecular weight of the sol is 10,000 And the glass transition temperature of the sol is- A heat-developable image recording material containing a polymer having a temperature of 30 ° C to 50 ° C. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7144693-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7381520-B2 |
priorityDate | 2001-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 417.