http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002302609-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
filingDate | 2001-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f38411f97c73a725baacae0123375f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b217f36df177807aff6e1f8ac4ba5a5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9378674a43fe23851a2ab348adf51115 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dd7577ece96f2866d175a87ca3af408a |
publicationDate | 2002-10-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002302609-A |
titleOfInvention | Thermoplastic resin composition |
abstract | (57) [Problem] To provide a thermoplastic resin composition excellent in moldability in blow molding, extrusion molding and the like. SOLUTION: A polytetrafluoroethylene-containing mixed powder (a) comprising polytetrafluoroethylene particles and organic polymer particles having an epoxy group is blended with a thermoplastic resin (b) such as a polyester resin. 270 ° C, angular frequency 1 to 10r The angular frequency at which the ratio G's / G'b of the storage elastic modulus G's of the resin composition to the storage elastic modulus G'b of the thermoplastic resin (b) alone in the dynamic viscoelasticity measurement at ad / sec is 3 or more. Is a thermoplastic resin composition. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108884324-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2012196983-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017122743-A1 |
priorityDate | 2001-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 99.