http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002293838-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 |
filingDate | 2002-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3282722fbcf9add861ec4f40cbc6e1f2 |
publicationDate | 2002-10-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002293838-A |
titleOfInvention | Soft acrylic copolymer, method for producing the same, and soft resin composition |
abstract | PROBLEM TO BE SOLVED: To provide a novel soft acrylic copolymer containing no halogen atom instead of a soft vinyl chloride resin, a method for producing the same, and a soft resin composition containing the copolymer. . SOLUTION: It consists of a copolymer of 40 to 70% by weight of methyl methacrylate and 60 to 30% by weight of n-butyl acrylate, and has a reduced viscosity of 0.9 to 3.0 dl / g and a glass transition point of 90 ° C. or less. And a soft acrylic copolymer having a tan δ at 20 ° C. of 0.07 or more. This copolymer is produced by suspension polymerization or the like. Further, the soft resin composition can be obtained by adding a plasticizer to the copolymer. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10851233-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006241274-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018168954-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10851234-B2 |
priorityDate | 2001-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 57.