Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_48ccd54a3001e53e9982db9a50929af0 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-91 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00706 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B18-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H02G1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16L1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H02G9-06 |
filingDate |
2001-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_63d11eb157cc92b729f007e53241b10d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_929dc1a06d7bcf844f4b6859e30bff15 |
publicationDate |
2002-10-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002291144-A |
titleOfInvention |
Filling material for underground power transmission lines |
abstract |
(57) [Abstract] [Problem] It has high heat conductivity, less breathing, Provide a filler excellent in fluidity and strength development. SOLUTION: For a mixture containing 30% by mass or less of cement and 70% by mass or more of coal ash, water and an admixture are added to adjust the flow value to 200 to 400 mm. Provide materials. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006069855-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2065902-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006143913-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008031638-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4490796-B2 |
priorityDate |
2001-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |