http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002268274-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2001-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7a980397a1ff73a2efbf0b70e9c731b8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d968c3c0865bad1316d61ae35056c663 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d0bb26c1c9fd35a294032bd5930a22e9 |
publicationDate | 2002-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002268274-A |
titleOfInvention | Toner manufacturing method |
abstract | (57) [Summary] (with correction) [Problem] To achieve both improvement of coloring degree and transparency and charging stability under high temperature environment, and excellent toner quality characteristics. Provided is a method for producing fine particles such as toner with high productivity. A binder resin for dilution and a charge controlling agent are mixed with a binder resin using a master batch kneading method in which a loss on drying at 110 ° C. after mixing and kneading a pigment and a dispersing resin is 0.01 to 1.0%. Knead at low temperature and crush and classify. In the kneading process, 70 A binder resin for dilution and a charge controlling agent are kneaded at a low temperature using a master batch having a loss on drying at ゜ C of 0.05% or less. It is preferred that the binder resin for dilution and the charge control agent be specified at a kneading temperature of 50 to 100 ° C. |
priorityDate | 2001-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links