http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002265703-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6dd74b20fbf2e0ebf10c7bfad4f6c8c5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3477 |
filingDate | 2001-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_483d4de4604cf7e0ddbe1ee6095e0c02 |
publicationDate | 2002-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002265703-A |
titleOfInvention | Flame retardant resin composition |
abstract | (57) [Problem] To provide a flame-retardant resin composition having the same flame retardancy, mechanical strength, and hardness as a rigid vinyl chloride resin material and not generating a halogen compound during combustion. The problem can be solved by a flame-retardant resin composition containing 45 to 100 parts by weight of a phosphorus-based flame retardant and 10 to 30 parts by weight of an isocyanuric derivative per 100 parts by weight of high-density polyethylene. Further, 1 to 5 parts by weight of hydrotalcite may be blended with respect to 100 parts by weight of high-density polyethylene. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014062159-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006506486-A |
priorityDate | 2001-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 41.