http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002265699-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-295 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B3-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate | 2001-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8656d853aa413db00bf294252c81a543 |
publicationDate | 2002-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002265699-A |
titleOfInvention | Thermoplastic resin composition |
abstract | PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition having excellent oil resistance and flame retardancy and excellent flame retardancy without using a halogen-based flame retardant or a phosphorus-based flame retardant as an essential component. The present invention provides a thermoplastic resin composition optimally used for covering electric wires or cables. SOLUTION: It contains the following (A) to (C), and (A) / (B) a weight ratio of 30/70 to 80/20, A thermoplastic resin composition wherein the content of (C) is 0.1 to 10 parts by weight based on 100 parts by weight of the total of (A) and (B), and (A) forms a continuous phase. (A): Polyolefin resin (B): Polyphenylene ether resin (C): Specific polyorganosiloxane |