http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002264025-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24D3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24D11-00 |
filingDate | 2001-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c621f7d78a802c0d63bbe77841929818 |
publicationDate | 2002-09-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002264025-A |
titleOfInvention | Polishing film |
abstract | PROBLEM TO BE SOLVED: To provide a polishing film which is suitably used for polishing an end face of an optical fiber connector, and which makes it easy to judge a wear state by use. SOLUTION: The base film 2 and the base film 2 are provided. Abrasive particles 5 and binder resin 6 even if formed on The above object is attained by providing at least one indicator layer 4 having a pigment 7 and a binder resin 8 on the polishing film 1 having a polishing layer comprising: |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020078868-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012106178-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016536151-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013500173-A |
priorityDate | 2001-03-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 43.