http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002227041-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01G1-04 |
filingDate | 2001-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_684a66104b059cf5c370c23f36dcc579 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2cb2585ad06f9cbe7288452ede2a1811 |
publicationDate | 2002-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002227041-A |
titleOfInvention | Method for producing polyester short fiber |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a high-quality polyester short fiber, particularly a polyester short fiber for papermaking, by stably and accurately cutting an undrawn polyester yarn immediately after spinning. I do. SOLUTION: After cooling and solidifying a polyester yarn melt-spun from a spinneret, the moisture content of the fiber bundle is adjusted to 3 to 50%. %, And immediately cut into a range of a cut length of 3 to 30 mm. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7051323-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019026983-A |