http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002226653-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c06ff00cc23d0d0c48233a171dccb984 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-02 |
filingDate | 2001-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b6eb5ad9874d39637e7ee6047d40907 |
publicationDate | 2002-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002226653-A |
titleOfInvention | Rubber-modified thermoplastic polymer composition |
abstract | PROBLEM TO BE SOLVED: To provide a rubber-modified thermoplastic polymer composition which suppresses transfer unevenness and is excellent in moldability and surface appearance. SOLUTION: The rubber-modified thermoplastic polymer composition contains a grafted rubbery polymer (A) in which a vinylic monomer is grafted on a rubbery polymer and an aromatic vinyl-based polymer. The composition is a capillary rheometer (temperature 20 (0 ° C.) at a shear rate of 500 / sec. 00 poise or more and at a temperature of 200 ° C., 25 to 1 The die swell ratio in the 00 / sec shear rate region was 1. 2 or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015003996-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006150950-A |
priorityDate | 2001-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 144.