http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002212348-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 |
filingDate | 2001-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2188341072597cb0d0d62f3a4606129 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_78238616d9cbcc7a9bbae8a5b266f61f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d1749b3a3d07fa459d6bdb06dfe6717 |
publicationDate | 2002-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002212348-A |
titleOfInvention | Extruded product made of olefin / aromatic vinyl resin composition |
abstract | (57) [Summary] (Modified) [Problem] To provide an extruded product excellent in heat-softening resistance, weather resistance and chemical resistance. (A) Melt flow ratio (MFR) measured at 200 ° C. and 5 kg with an aromatic vinyl compound monomer unit content of 1 to 95 mol% is 10 g / 10 mi. n or less (however, excluding 0 g / 10 min), 97 to 10 parts by weight of the aromatic vinyl compound-olefin random copolymer and the melting point of the crystal (B) are 100 ° C. or more, and the melting energy of the crystal is 80 J / g or more. And 200 ° C, 5k The melt flow ratio (MFR) measured under the condition of g is 1 It is an extrusion molded product of an aromatic vinyl compound-olefin random copolymer resin composition comprising 3 to 90 parts by weight of a crystalline α-olefin polymer of 0 g / min or less (excluding 0 g / 10 min). A molded article having a shrinkage in the extrusion direction of 10% or less when the article is left at 120 ° C. for 1 hour. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006517477-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4644656-B2 |
priorityDate | 2001-01-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 82.