http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002205457-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-326 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-322 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y35-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-54 |
filingDate | 2001-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98c24fb0ea36dce2df4104ad5f40b629 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aaa64785d9d59b724fd6f2a151a52c8d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a0f9fe80de4170d0a69a74f43592915 |
publicationDate | 2002-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002205457-A |
titleOfInvention | Method for measuring physical properties of pore caused by liquid composition, liquid composition, ink set, method for forming colored portion on recording medium, and ink jet recording apparatus |
abstract | PROBLEM TO BE SOLVED: To provide a method for measuring a physical property value derived from a liquid composition which makes it possible to obtain a higher quality ink jet recorded matter having particularly excellent coloring properties, a liquid composition, an ink set, and a recording medium Provided is a method for forming a colored portion on an ink jet recording apparatus. SOLUTION: After pretreating a liquid composition containing at least fine particles and a solvent in the order of the following (1) to (3), A method for measuring a liquid composition comprising a step of measuring the pore properties of fine particle aggregates formed from the liquid composition by vacuum degassing at 20 ° C. for 8 hours by a nitrogen adsorption / desorption method: (1) The above liquid composition The material is dried at 120 ° C. for 10 hours in an air atmosphere, (2) Dry the above dried product by evaporating almost the solvent. After raising the temperature from 20 ° C. to 700 ° C. for 1 hour, 700 (3) After sintering for 3 hours, the baked product is gradually returned to normal temperature, and the baked product is powdered. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015193174-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7427130-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8220899-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8016404-B2 |
priorityDate | 2000-10-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |