http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002187713-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_18be3eacd550050c2642699ea6d8ae44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d6af5256018a43c472efcbffc08f93cf |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B39-02 |
filingDate | 2000-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba8ba078530b838afc79d9772caa6cba |
publicationDate | 2002-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002187713-A |
titleOfInvention | Method for producing artificial zeolite |
abstract | PROBLEM TO BE SOLVED: To provide a novel method for producing an artificial zeolite capable of preventing or reducing elution of harmful substances such as CN compounds and hexavalent chromium from the produced artificial zeolite. SOLUTION: A mixed slurry of fly ash and an aqueous solution of sodium hydroxide is subjected to hydrothermal treatment in a state where an oxidizing agent such as hydrogen peroxide is added thereto. Fe 2+ by washing with a washing liquid of a mixture of l 2, etc. Apply ions. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-105189353-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014168049-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-6036993-B2 |
priorityDate | 2000-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.