http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002172676-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b19eaa8e535da4e4bceed99917a68153 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2000-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_233e71969a29f076c4688442c02246b3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9340e27a44e9d71ee844ac53f10603a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e81568e6853b5567b7b3facb252826ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82f0915996ccd79621fef34099ee672e |
publicationDate | 2002-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002172676-A |
titleOfInvention | Polymer sheet, method for producing polymer sheet, and liquid crystal display device |
abstract | (57) [Summary] [PROBLEMS] Excellent heat resistance, excellent smoothness of sheet surface, To provide a method for producing a polymer sheet having few projections. SOLUTION: The glass transition point is 150 ° C. or higher, the number average molecular weight (M n ) is 11,000 to 25,000, Melt viscosity (330 ° C, 5min, 50kg: Die 1m a polymer sheet having a thickness of 70 μm or more and 1000 μm or less produced by melting and extruding a polyether sulfone having a m diameter of 10 mm) of 1700 to 2300 Pa · S with a T die or a coat hanger die. Manufacturing method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8025997-B2 |
priorityDate | 2000-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.