http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002172636-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-46 |
filingDate | 2000-12-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f39e76752d0043958f14fa0830fce46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce361440fe3a05d0665ff351efaaa761 |
publicationDate | 2002-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002172636-A |
titleOfInvention | Method for producing aramid molding |
abstract | (57) [Problem] An object of the present invention is to provide a method for producing a light and strong aramid molded article. SOLUTION: A powder composed of a high molecular weight substance mainly composed of an aromatic polyamide and having an average particle diameter of 1 to 500 µm is dispersed in a mixed solution of water (A) and an organic solvent (B). A slurry (C) having fluid formability is formed, and then the slurry (C) is charged into a mold, and the water and the organic solvent are released from the mold by heating to bind the powders together. . |