http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002161137-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b19eaa8e535da4e4bceed99917a68153 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-12 |
filingDate | 2000-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bcaccd985b75f5b8d8c7c1f8970d24a9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4aaab93d0ffae6e6e1e8adc7b3103cf |
publicationDate | 2002-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002161137-A |
titleOfInvention | Block copolymerized maleimide resin and method for producing the same |
abstract | (57) [Problem] To provide a maleimide resin having flexibility, high strength and high heat resistance, and a method for producing the same. SOLUTION: A maleic acid analog monomer and / or a maleic anhydride analog monomer and a diamine are mixed without using a solvent, and the mixture is heat-treated at 80 to 200 ° C. to obtain a continuous general Two types of maleimide-based resin oligomers (a) and (b) each having a repeating unit represented by the formula (1) and the general formula (2), or a diamine, maleic acid or maleic anhydride (c) ), And the mixture is mixed without using a solvent so as to have a predetermined weight ratio, and then heat-treated at 80 to 200 ° C. Embedded image Embedded image |