http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002160338-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-733 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B5-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 2000-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e8f26732a8e58463c58ffea4e0d2a57f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc26548af70a21fbd2afdc53acb0039d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2fe2a602a4e134c47e63cab8faae9b77 |
publicationDate | 2002-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002160338-A |
titleOfInvention | Polyester film |
abstract | PROBLEM TO BE SOLVED: To provide a high productivity, a small amount of foreign substances mainly composed of oligomers deposited on the surface after film formation, and particularly excellent in electromagnetic conversion characteristics when a metal-deposited thin film type magnetic recording medium is used, and a dropout. To provide a polyester film with a small amount. SOLUTION: One surface of a layer A made of a polyester resin having an intrinsic viscosity of 0.55 or more has an average particle diameter of 10 to 50. nm and a continuous film C containing 0.5 to 30% by weight of inert particles C having a volume shape factor of 0.1 to π / 6, and a film surface roughness WRa on the film C side of 0.1 to 30% by weight. 4n m, and the number of foreign substances deposited on the film C when the film is held at 120 ° C. for 30 minutes is 1,000 / mm 2. A polyester film characterized by the following. |