http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002160335-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 2001-09-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e5814487e1feca85b4f235e05d4ade49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba7a801694bf417e7fa671e3beca4573 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f59b832b1351129540565089da58d6f8 |
publicationDate | 2002-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002160335-A |
titleOfInvention | White polyester film for metal plate lamination, film-laminated metal plate and metal container |
abstract | (57) [Summary] [PROBLEMS] To be excellent in heat resistance, to be able to stably coat the surface of a metal plate even after heat treatment in a can making process, etc., and to be excellent in concealing properties, barrier properties, and corrosion resistance. To provide a polyester film. SOLUTION: A white biaxially stretched polyester film having the following characteristics: (a) A layer made of polyester having a melting point of 240 ° C to 260 ° C and containing 5 to 30% by weight of titanium dioxide; Is a two-layer structure of A / B composed of a polyester B layer having a temperature of 210 ° C. to 235 ° C .; The dimensional change rate when the heat treatment is performed for 2 minutes in an atmosphere of ° C. is 2% or less. |
priorityDate | 2000-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |