http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002148866-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-097 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2001-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df4dfa72151c0f9c0bba372113296acf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aed6464ea66be9adb0365541d5269990 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7738ec9e6d0124421bde94b6d102028a |
publicationDate | 2002-05-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002148866-A |
titleOfInvention | Electrostatic image developing toner and method of manufacturing the same |
abstract | (57) [Solution] As a heat roller fixing method, a so-called oil-less method that enables fixing without using an offset prevention liquid, and a spherical shape to a substantially spherical shape capable of obtaining a developed image of excellent quality. It is desired to provide a toner for developing an electrostatic charge image comprising a polyester resin and a method for producing the same. SOLUTION: This is an electrostatic image developing toner containing at least a binder resin and a colorant. The binder resin is a polyester resin, and the outflow starting temperature Tfb of the toner by a constant load extrusion type capillary rheometer is 90 ° C. or higher, and 12 0 ° C. or less, T1 / 2 temperature exceeds 120 ° C., 160 ° C. or less, outflow end temperature Tend is 130 ° C. or more, 170 ° C. or less, and the following equation: Average circularity = (a circle having the same area as the projected area of a particle) Perimeter) / The average circularity defined by (perimeter of particle projection image) is from 0.97 or more to a spherical shape or a substantially spherical shape. Further, the toner having such characteristics can be suitably manufactured by adding an alcohol solvent and inverting the phase with a low shear of 0.2 to 5 m / s. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7113723-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012255083-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004226572-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4761206-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004004387-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7862974-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007171927-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004271919-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008020475-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005025144-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010282209-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8361690-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004286824-A |
priorityDate | 2000-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 128.