http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002145911-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8cde4f2bd60df7888c8040bdfcc8a5d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-38 |
filingDate | 2000-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0dc77284f86461ac06447aae334cc0c9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3730e36b0057fb6dee591de675af53c |
publicationDate | 2002-05-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002145911-A |
titleOfInvention | Emulsion polymerization method for vinyl compounds |
abstract | (57) [Problem] To provide a method for producing an emulsion polymer of an ethylenically unsaturated monomer having excellent polymerization stability and good mechanical stability. SOLUTION: When emulsion polymerization of an ethylenically unsaturated monomer is carried out, (A) an ethylenically unsaturated monomer 100 0.05 to 5 parts by mass with respect to parts by mass of the emulsifier, 0.05 (B) a polyvinyl alcohol-based resin having a saponification degree of 60 mol% or more and a 4% aqueous solution viscosity at 20 ° C. of 2.0 mPa · s or more; With ethylenically unsaturated monomer 100 Polymerization is carried out by adding to an aqueous solution dissolved so that the addition amount is 2 to 20 parts by mass with respect to parts by mass. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006123948-A2 |
priorityDate | 2000-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 92.