http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002120341-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-06 |
filingDate | 2000-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_073ffbdc09e860f78b93785cccafa0a9 |
publicationDate | 2002-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002120341-A |
titleOfInvention | Composite foam sheet and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a foamable sheet which can be formed to have a small thickness, can achieve a high expansion ratio, is excellent in light weight, and has bending rigidity and compressive rigidity. And a composite foam sheet excellent in dimensional stability and a method for producing the same. SOLUTION: The composite foamed sheet of the present invention is obtained by laminating and integrating a sheet-like material on one surface of a foamed sheet obtained by foaming a polyolefin resin having a maximum spreading ratio at 180 ° C of 8 or more. The foam sheet has an expansion ratio of 10 5050 cm 3 / g and the aspect ratio (Dz / Dxy) of the bubble is 1.2 or more. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006028255-A |
priorityDate | 2000-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 66.