http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002114886-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F291-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F279-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-10 |
filingDate | 2001-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_148d8a60d2f62421d34b8e3d7087bfa2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c23281a974fcadf3c63537cb870d4081 |
publicationDate | 2002-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002114886-A |
titleOfInvention | Rubber-modified copolymer resin composition |
abstract | (57) [Summary] [PROBLEMS] To obtain a molded article having both impact resistance, oil resistance and transparency. SOLUTION: It has 17 mol% of 1,2-vinyl bonds, A rubber-modified copolymer resin obtained by continuous bulk polymerization of styrene, methyl methacrylate, and acrylonitrile in the presence of a styrene-butadiene copolymer rubber having a styrene / butadiene weight ratio of 35/65, and a plasticizer are essential. A rubber-modified copolymer resin composition as a component, having a toluene insoluble content at 25 ° C. of 4 to 22% by weight, a toluene swelling index at 25 ° C. of 11 to 19, and a toluene insoluble content. / The swelling index is 0.20 to 1.20% by weight. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2006062315-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100690344-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7863359-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101072803-B |
priorityDate | 2001-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 104.