Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f95e92e0fb1e1198b34494bd59d56f2e |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-24 |
filingDate |
2000-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_360e7b1ca5cc0acd9f319b63632ee321 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b93f1a3b805d720afbf7d26189fa38c9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d834bf2ab1906573aaf59e42549794fa |
publicationDate |
2002-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002110224-A |
titleOfInvention |
Activation method of sealed nickel-metal hydride battery |
abstract |
(57) [Abstract] [Purpose] This is a method of forming a sealed nickel-hydrogen storage battery. By activating the battery without repeating charge and discharge, a battery with high rate discharge characteristics and excellent discharge capacity can be efficiently manufactured. provide. A sealed nickel-hydrogen storage battery provided with a hydrogen storage alloy electrode storing hydrogen has a temperature range of -20 to 80. A temperature raising / lowering cycle operation is added at 0 ° C. Further, the above-mentioned heating / cooling cycle operation is combined with charging at 10 ° C. or lower. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4706163-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013118661-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2013118661-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004281195-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9865872-B2 |
priorityDate |
2000-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |