Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate |
2000-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2309d5095a2d9a7d5a45c67124b90e33 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_15e0eea87a144769ee0bdd9e71b820a3 |
publicationDate |
2002-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002105753-A |
titleOfInvention |
Method for producing polyester fiber |
abstract |
(57) [Problem] To provide a method for producing a polyester fiber excellent in spinnability with few yarn breakage in high-speed spinning. A method for producing a polyester fiber using a polyester obtained by using a specific amount of a titanium compound and an antimony compound as a polymerization catalyst when spinning the polyester at 5500 m / min or more. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015029316-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004244770-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004238769-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9732443-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190140958-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102144109-B1 |
priorityDate |
2000-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |