http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002105553-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_25ba42e5f214f100f81e5e2016f045ce |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B5-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B61-00 |
filingDate | 2000-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b420aaff397306149d1a4ed6f9355c57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b6667c5c640c1b54c2f6fc02fcc123f |
publicationDate | 2002-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002105553-A |
titleOfInvention | How to recover tellurium |
abstract | (57) [Problem] To recover tellurium from copper telluride generated in a treatment process of anode mud in copper electrolytic refining at low cost. SOLUTION: The weight ratio of copper telluride is 0.26-1. By adding and heating 20 times the amount of sulfur, the tellurium of copper telluride is replaced with sulfur, and a mixture of copper sulfide and tellurium is generated. After evaporating and separating excess sulfur from the mixture and heating the mixture to 200 to 1000 ° C. under reduced pressure, only tellurium is vaporized, and high-purity tellurium is aggregated in the cooling part. Copper sulfide, a by-product, is reused as a raw material for smelting copper. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104445101-A |
priorityDate | 2000-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 53.