http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002103833-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C25F3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N1-083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41N3-034 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41N1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22C21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-16 |
filingDate | 2000-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03f65ed85e5c4a265e682c618b04722a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c19c2335ba2dfc868e02b4e44b0f1b36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79318b45e514ef37f34cc1b08dc226dc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5964d861b26a8a4d16c43918d4083ca7 |
publicationDate | 2002-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002103833-A |
titleOfInvention | Method for producing a lithographic printing plate support |
abstract | (57) [Abstract] (with correction) [Problem] To suppress production of severe ink stains and to produce at low cost even when using a raw material in which trace components are segregated and aluminum crystal grains are exposed. Provided is a method for producing a lithographic printing plate support that can be performed. SOLUTION: The manufacturing method for manufacturing a lithographic printing plate support from an aluminum alloy plate W, wherein the aluminum exposed on the surface of the aluminum alloy plate W has a certain size, When the electrochemical surface-roughening treatment is performed, the abundance of Cu exposed on the surface of the aluminum alloy plate becomes 5 (mm 2 / m 2 ) or more, and at least the following (1) and (2) A method for producing a lithographic printing plate support, characterized by sequentially performing each of the processes comprising the steps of: (1) 1 to 300 C / d using alternating current in hydrochloric acid solution a hydrochloric acid electrolytic treatment step of performing an electrochemical graining treatment with an amount of electricity of m 2 . (2) A nitric acid electrolytic treatment step of performing an electrochemical surface-roughening treatment using an alternating current in a nitric acid solution. |
priorityDate | 2000-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 379.