http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002103019-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5d04736b0b882a4f5a1e0e0e4cd8cbb |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12R1-865 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07K14-39 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D27-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12N15-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12Q1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22D46-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N33-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C12N1-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N33-50 |
filingDate | 2000-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_829263e95a46ffac3e795e48edb32006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1fd401a6bddab69ce3d34968ef7b73ac http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9bcdbc9d74b46a0468180d5e7bf7087a |
publicationDate | 2002-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002103019-A |
titleOfInvention | Metal casting method, metal casting apparatus and ingot |
abstract | (57) [Problem] To provide a metal casting apparatus capable of obtaining an ingot of good quality with good production efficiency. SOLUTION: A casting control means 19 instructs an opening / closing stopper raising / lowering mechanism 9 to open an injection port 7 to start injection of a molten metal 5 into a mold 4. It is determined that the inner surface is covered based on a change in the temperature or the temperature gradient of the cooling plate 2, etc., the electromagnetic valve 17 is turned on, the on-off valve 16 is opened, and cooling water is sprayed from the spray nozzle 12 to the cooling plate 2, After a lapse of a predetermined time from the start of pouring, the injection port 7 is closed, assuming that solidification has progressed to the vicinity of the injection port 7. After that, when the cooling end condition is achieved, the injection of cooling water is stopped, and the ingot removal condition is When this is achieved, the cooling plate elevating mechanism 14 is operated to lower the cooling plate 2 and take out the ingot 5 ′. Then, the cooling plate 2 is raised and attached to the lower part of the mold body 3. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009226428-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4591528-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101367119-A |
priorityDate | 2000-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962 http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635 |
Total number of triples: 27.