http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002097335-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F291-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 |
filingDate | 2001-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e13339b57f96fd31410c43f02418680f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7d5a739390dcfca1890e0cc1905bab7b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a7c69c61d1e3675decb7344776fb269a |
publicationDate | 2002-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002097335-A |
titleOfInvention | Rubber-modified aromatic vinyl copolymer resin composition |
abstract | (57) [Problem] To provide a rubber-modified aromatic vinyl copolymer resin composition having transparency and practical properties, particularly excellent in Charpy impact strength and falling weight impact strength. A rubber-modified aromatic vinyl copolymer resin containing a styrene-butadiene block copolymer having a specific glass transition point as dispersed particles in an amount of 99 to 80% by mass, a hydrogenated coumarone resin, an MBS resin, and a styrene resin. A composition comprising 1 to 20% by mass of at least one resin selected from butadiene-based block copolymer resins. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7145271-B1 |
priorityDate | 2000-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 200.