http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002085546-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8aa118fbfa85a6e0cc8c13a8afca19ab |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L27-00 |
filingDate | 2000-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_056364119bda3a00c87d70d9389c30a7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3da619e68a680a05ef682e7dea309e7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_04789249a0cc666a076b0301f32f4f6e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ece0f48e7e0e37ab88622f9696b1e04 |
publicationDate | 2002-03-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002085546-A |
titleOfInvention | Bioactive cement composition |
abstract | PROBLEM TO BE SOLVED: To provide a bioactive cement composition which can be directly bonded to natural bone, has high mechanical strength, has good durability in a living body, and has good workability. It is. SOLUTION: It consists of Ca-containing glass or crystallized glass, silane-coupled bioactive powder, polymethacrylate-based powder, methacrylate-based monomer, polymerization initiator, and polymerization accelerator, The amount of the silane coupling agent attached is 0.01 to 0.10% by mass relative to the bioactive powder. |
priorityDate | 2000-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |